Description
>>> GebrAnw-Dental-Base-Alloy-Adorbond+.pdf <<<
| Type: | Gold-reduced metal-ceramic alloy on the gold basis, type 4 (extra hard)
 acc. DIN EN ISO 22674  | 
| Colour: | white | 
| Applicable scope: | Inlays, Onlays | ● | 
| Crowns | ● | |
| Small bridges | ● | |
| Large-span bridges | ● | |
| Milling, cone and attachment works | ● | |
| Modeling casting | ● | 
| Composition: | Au | 51,60 | 
| (mass fraction in %) | Pd | 38,40 | 
| Ir | 0,05 | |
| Ru | 0,05 | |
| In | 8,40 | |
| Ga | 1,50 | 
| Technical specifications: | Density in g/cm³ | 13,8 | 
| Vickers hardness HV 5/30 | (s)220 (n)220 (a-n)230 | |
| Yield strength Rp0,2 in MPa | (s)470 (n)530 (a-n)560 | |
| Elongation at break in % | (s)31 (n)30 (a-n)29 | |
| Average linear CTE 25 – 500 °C in 10-6 K-1 | 13,5 | |
| Average linear CTE 25 – 600 °C in 10-6 K-1 | 13,8 | |
| Elastic modulus in GPa | 110 | |
| Melting interval in °C | 1200 - 1310 | 
| Processing: | Preheating temp. of the casting moulds in °C | 900 | 
| Casting temperature in °C | 1460 | |
| Crucibles | Ceramic | |
| Curing | 500°C/15min | 
| Suitable solders: | Joints before ceramic firing | AL 1060 W | 
| Joints after ceramic firing | AL 750 | 
1) Brief description:
s – self-curing, n – after ceramic firing, a-s – curing from s condition
a-n – curing from n condition
2) All information about cured condition is given according to the alloy:
– Oxide firing 10min/ 960°C + 4x4min/ 960°C for yellow conventional bonding alloys
– Oxide firing 10min/ 980°C + 4x4min/ 980°C for white conventional bonding alloys
– Oxide firing 10min/ 800°C + 4x4min/ 800°C for LFC-systems
Corresponding data are true under these conditions only.
3) The ceramic firing should be carried out according to the manufacturer's instructions.

Reviews